Asian Paints Emporio PU 50% Glossy Clear 1Ltr
Asian Paints Emporio PU Glossy - A Semi-Gloss (50% Gloss) Finish coat for Interior and Exterior Wood.
Read our Security Policy
Fast Deliveries
Easy Returns
Emporio PU (Polyurethane) is an excellent choice when you want to protect expensive Teak, Walnut, Wenge or other exotic woods from the elements. It has good UV resistance and excellent sealing properties against water, moisture and humidity. PU retains it finish over prolonged exposures to UV. PU Matt and Glossy finishes for wood.
Emporio Clear PU Finishes are used to protect wood while retaining its original grains by creating a transparent polyurethane film over the wood.
Emporio PU is available in Glossy, Matt and Sealer variants in both clear and opaque finishes.
Asian Paints Emporio PU is a fully imported wood finish product from the masters of wood finishes in Italy - Renner.
Emporio PU has the advantages of
- High Clarity
- Abrasion Resistance - Extremely durable
- Superior Film Toughness - High Impact Resistance
- Excellent Scratch Resistance
- Faster Drying time
How to apply PU coatings to wood
Materials Required
- Woodtech Emporio PU Clear Sealer
- Woodtech Emporio PU Clear Top coat - Glossy - This product
- Woodtech Emporio PU Clear Top coat - Matt - This product
- Wood stains, if required.
- Exterior Wood Stains, if required
- Dent Fillers
- Emporio PU Thinner
- Compressor for spray.
- Pilot Spray Gun 250ml Cup or
- Pilot Spray Gun 500ml Cup
- Dry Sanding Aloxite Paper 80, 120, 180
- Open Coated Dry Sanding Paper - Deerfos Non Loading (Babloo Paper) - 220, 320
- Wet Sanding Paper 320, 600, 800, 1000
- 3M Hand Pads for Sanding
- Cotton Waste.
- Filter Cloth.
- Masking Tape.
- Dust Mask
- Face Mask to prevent inhalation of spray.
- Gloves
- Eye glasses.
Application
- Prepare the wood by dry sanding with emery grit 80 to smooth the grains and undulations on the surface. Sanding should be done along the grain.
- Look for dents, cracks and aberrations on the surface and correct them. Dents and similar aberrations can be repaired using transparent or pigmented wood/dent fillers. Fillers can be pigmented using wood stains and powder pigments to get the desired results. Discoloured areas can be coloured to match the wood using wood stains and powdered pigments. This is an informative article on how to stain wood.
- Once major imperfections are removed, dry sand with emery grit 120 to get a smoother finish.
- Switch on the compressor to get the required PSI. (Here is an excellent article on how to spray paint using a paint gun and a compressor). Connect the spray gun to the compressor.
- Wipe clean the surface to be sprayed using a dry cotton cloth.
- The Sealer can be tinted or transparent depending on the desired final finish.
Pre-preparation For Porous woods
- Mix the Sealer base and hardner in the given proportion without adding thinner. (All Mixes must be consumed within the prescribed pot life)
- With a muslin/cotton cloth apply sealer mix along the grain on to the entire surface maintaining uniform thickness.
- After the sealer has completely cured and hardened, sand the flat surfaces with 180 grit free cut/ open cut emery using an emery trowel. For uneven, round, carved etc surfaces, 3M hand pads/scotch brite hand pads equivalent to 180 grit can be used. All excess sealer must be sanded and removed completely to get a smooth uniform surface. Wipe the thus surface clean.
- The rest of the procedure is the same as for regular woods.
For Regular woods
- Mix Sealer base and hardner along with 10% - 15% thinner. Pour mix into the spray gun.
- Spray the sealer onto the surface.
- Clean the spray gun.
- Wait for sealer to cure and harden.
- Sand with emery/hand pad grit 600. Wipe clean.
- Additional coats of sealer can be applied for a smoother finish.
- Mix Top coat (Matt or Glossy or Mix a of the two) base and hardner in the given proportion along with 10% - 15% thinner. Pour mix into the spray gun.
- Spray mix onto the entire surface.
- Wait for top coat to cure and harden.
- Sand with emery/hand pad grit 800. Wipe clean.
- Spray a second coat of the top coat.
- Wait for top coat to cure and harden.
- In case of gloss finish, additional top coats can be added by sanding with 1000 grit emery between coats.
- Gloss top coats can be further buffed using rubbing compounds to get a high gloss finish.
Notes
- If the wood is previously coated, remove the coating by scraping and a paint remover. Ensure the paint remover has completely evaporated before coating.
- Ensure exterior woods are coated from all sides.
Product Technical Details
- Mixing Ratio : Resin : Hardner : Thinner - 100 : 100 : 15 By Volume
- Recommended Thinner : Emporio PU Thinner
- Pot Life : 90Minutes
- Flash Off Time : 15 Minutes
- Recoating Time : 3-4 Hours
Data sheet
- Material
- Polyurethane
- Finish
- High Gloss
- UV Resistant
- Moderate UV resistance
- Non-Yellowing
- Yes
- Scratch Resistant
- Excellent
- Water Resistance
- Excellent
- Coverage
- 70 - 80sqft / ltr / coat
- Colour
- Clear
- Clarity
- Excellent
- Recoating Time
- 2-3 Hours
- Method of Application
- Spray
- Pack
- 2 Part - Resin + Hardner